因为现有的氯系列焊剂腐蚀性太强,所以存在必须用水清洗钎焊部位以及焊接后发生腐蚀等问题。但是本产品属于氟化物系焊剂,没有腐蚀性,所以也不需要用水清洗钎焊部位。
|
Because existing chlorine-based flux products havestrong degrees of corrosiveness, there can be problems involved with thebrazing area being required to be washed with water, and the resultant residualcorrosiveness. This product eliminates the need to wash the brazing area withwater, because it is a fluorine-based flux without any corrosiveness.
Product Name | Melting Temperature(oC) | BULK DENSITY(g/l) | Usage |
TAF-3 | 475±15 | 550~850 | Where a clad is not used Where the gap between the welding surfaces is wide |
TAF-5 | 525±15 |